TP027 – Development of Very High Strength Copper Alloys with Resistance to Hydrogen Embrittlement and Stress Corrosion Cracking

TP027 – Development of Very High Strength Copper Alloys with Resistance to Hydrogen Embrittlement and Stress Corrosion Cracking

La description:

This paper details the development of Hiduron® 220 (formerly Marinel 220) – specifically the control of the microstructure to achieve optimum mechanical properties. This alloy provides improved performance over Cu-Ni-Sn, particularly with respect to hydrogen embrittlement and stress corrosion cracking.

 

Project Overview:

  • Market Sector: All
  • Authors: C.Tuck
  • Company: Langley Alloys
  • Télécharger: Download pdf